OK (I’m the same guy who posted with the petg not sticking) Before Yesterday I bought overture petg and I was deceived because I had all kinds 1f issues… But then I tried to put the bed at 90C and the nozzle at like 280 ant it worked… How come i have to print this hot 🔥?
Is there a way you can confirm your bed or nozzle temps? I know for the nozzle that’s a really difficult thing to do, it’s so small to be able to check with anything.
I ask because with your unexpected crash the other day from your post history, I wonder if your main board has glitched.
A 90c bed shouldn’t melt petg I’d think, so something is definitely weird there.
Might be worth trying to reflash your firmware in case the glitch isn’t hardware.
What other mods have you done to your printer besides spring spacers?
When you level the bed, is it manually and with a piece of paper to help gauge the distance?
These things have so many places something can go off that it’s really difficult to help troubleshoot without being there. Hopefully something in this post helps you out.
Could also be the heat sensor is faulty, damaged wiring, etc. When I compare them, the reported number can be off by quite a bit from the real temperature .
For the crash my hotend just untightened lowering it lower than the bltouch. I use klipper now so the mainboard firmware akaik isn’t responsible for a lot. I have done A LOT of mods which I will list in a reply. For manually level the bed, I just probe 5p times my bed with abl, look at the graph and adjust the knobs in consequence…
Yeah I know it’s hard to troubleshoot without being there,trust me,trust me…
Thanks for your help I guess my filament is better at 280C ¯_( ツ )_/¯
So for the mods:
All in one rear mounted electronics box by Teaching Tech. Glass bed. Skr mini e3 v2. Sprite pro dd extruder. Klipper. Metal bed knobs and springs. PETG printed rear left tension remover. Crtouch. Ikea lack enclosure (not completely done YET). Others I might have missed so I guess it’s not important ¯_( ツ )_/¯
Ok, yeah, forget the paper as far as regular leveling goes with the cr touch. Have you tried confirming your z offset since you changed the nozzle? If you haven’t, it should be fine every time you do something to the hotend.
Also make sure your heat block isn’t stripped out. I had a bitch of a time printing for a while only to discover I had overtightened my middle and stripped out the threads in the heat block. After I replaced it I had consistent good prints again.
Check your thermistor and do PID tuning if you havent already. Your temps are high, but exact number doesnt matter if it works for you. You can see how stable is temperature curve while doing PID. Maybe print temp tower and post picture here
I already printed a temp tower and NO temps from 220 to 250 worked well
I guess you did PID and checked thermistor. Is your part cooling fan insanely powerful?
I ran a couple temp towers with the overture petg and I found 270-275c nozzle/80c bed had the most desirable results. 0.6 nozzle 0.15 layer height. also with the sprite pro.
I printed a couple pretty pieces before I started to get burnt crusty bits showing up in my prints so take this with a grain of salt. maybe due to me changing layer height to 0.14 without further testing.
Wow, exactly like me
This isn’t far off from where I print PETG with a stainless nozzle for 125mm/s. If you’re using a brass nozzle and not pushing speeds then it seems high.
Have you PID tuned it?
Ooh I might PID TUNE it buuut soon I want to go with a stainless steel nozzle. So you know… I will even go with a high flow one.